Top 6 - Adhesives for Heat Transfer
Supreme 18TC ONE PART, NASA LOW OUTGASSING EPOXY Click to request TDS for Supreme 18TC EP30TC TWO PART, ROOM TEMPERATURE CURING EPOXY Lower viscosity, good ow properties • Meets NASA low outgassing speci cations • Exceptional compressive strength Click to request TDS for EP30TC Not premixed & frozen • Cryogenically serviceable • Withstands 1,000 hours 85°C/85% RH Thermal conductivity, 75°F Volume resistivity, 75°F Service temperature range Abrasion resistance, CS-17 wheel, 1,000 cycles 18-20 BTU•in/ft²•hr•°F >10 14 ohm-cm -100°F to +300°F 54.1 mg Thermal conductivity, 75°F Volume resistivity, 75°F Service temperature range Tensile lap shear strength, aluminum to aluminum, 75°F 22-25 BTU•in/ft²•hr•°F >10 14 ohm-cm 4K to +400°F 2,200-2,400 psi