Top 6 - Adhesives for Heat Transfer
EP3UF ONE PART EPOXY FOR BONDING & UNDERFILLS Click to request TDS for EP3UF EP48TC TWO PART, NASA LOW OUTGASSING EPOXY Low coe cient of thermal expansion • High bond strength • Paste viscosity Click to request TDS for EP48TC Not premixed & frozen • Rapid curing with versatile cure schedules • Meets NASA low outgassing specifications Thermal conductivity, 75°F Volume resistivity, 75°F Service temperature range Viscosity, 75°F 9-10 BTU•in/ft²•hr•°F >10 14 ohm-cm -60°F to +300°F 10,000-40,000 cps Thermal conductivity, 75°F Volume resistivity, 75°F Service temperature range Tensile modulus, 75°F 20-25 BTU•in/ft²•hr•°F >10 14 ohm-cm -100°F to +300°F 600,000-700,000 psi