X5SC One Part Elastomeric System X5SC

Single component silver filled elastomeric adhesive, coating. Excellent electrical conductivity. Highly effective for shielding. Cures at room or elevated temperatures. Paste viscosity. Superior thermal conductivity. Performs well when subjected to thermal cycling, vibration. Serviceable from -80°F to +250°F.

X5TC One Part Elastomeric System X5TC

One part, thermally conductive adhesive offers convenient handling and application. Material is very thick but simultaneously very flowable. Relatively fast curing. Excellent electrical insulator. Good peel and shear strength properties. Well suited for bonding dissimilar substrates. Serviceable from -80°F to +250°F.