EP114 Two Component Epoxy EP114

Two component nanosilica filled epoxy for potting, coating and sealing. Optically clear. Low shrinkage. Superior electrical insulation properties. Toughened system. Successfully tested for 1,000 hours 85°C/85% RH. Serviceable from -100°F to +450°F.

EP121CL Two Part Epoxy System EP121CL

Low viscosity epoxy with an extraordinary long open time. Superior dielectric strength. Impressive optical clarity. Excellent chemical resistance. Serviceable from -80°F to +500°F.

EP121CL-LO Two Part Epoxy EP121CL-LO

NASA low outgassing approved two component epoxy. Low viscosity system. High dielectric strength. Optically clear. Withstands 1,000 hours 85°C/85% RH. Shore D hardness 80-90. Serviceable from -80°F to +500°F. Long open time at room temperature.

EP125 Two Component Epoxy EP125

Structural epoxy adhesive resists temperatures up to 500°F. Exceptional durability and flexural strength. High adhesion to metallic and non-metallic substrates. Heat curable system. Tg +240°C. Special two part epoxy with very long working life. Excellent compressive strength. Service operating temperature range from -80°F to +600°F.

EP126 Two Component Epoxy Compound EP126

Two part toughened epoxy system. Capable of continuous service at 500°F. 100% reactive. Unmatched durability. Outstanding chemical resistance. Robust physical strength profile. Dimensionally stable. Machineable. Withstands rigorous thermal cycling. Service operating temperature range from -80°F to +500°F.

Two Part Epoxy EP126TK EP126TK

Two part toughened epoxy system. Capable of continuous service at 600°F. 100% reactive. Unmatched durability. Outstanding chemical resistance. Robust physical strength profile. Dimensionally stable. Machineable. Withstands rigorous thermal cycling. Service operating temperature range from -80°F to +600°F.

EP13 One Part Epoxy System EP13

One component, heat curable epoxy adhesive. Serviceable from -60°F to +500°F. Paste viscosity. High tensile shear and compressive strength. Chemical resistant. Machinable.

EP132 Two Part Epoxy EP132

Two part high temperature resistant epoxy system. Capable of service up to 550°F. 100% reactive. Unmatched durability. Outstanding electrical and physical strength properties. Service operating temperature range from -60°F to +550°F.

EP13LTE One Part Epoxy EP13LTE

One component, heat curable epoxy adhesive. Serviceable from -60°F to +500°F. Paste viscosity. High tensile shear and compressive strength. Chemical resistant. Machinable. Low coefficient of thermal expansion. Meets NASA low outgassing standards.

EP13SPND-2 One Part Heat Cure Epoxy EP13SPND-2

Non-drip single component adhesive. Will not flow when cured. Serviceable up to +500°F. Electrically insulative. Withstands 1000 hours 85°C/85%RH. Excellent bond strength properties.