EP37-3FLFAO Flexible, low viscosity, thermally conductive epoxy. Meets NASA low outgassing specifications. Superb electrical insulator. Good physical strength. Chemical resistant. Long working life. Withstands 1,000 hours 85°C/85% RH. Guards against mechanical shock and vibration. Excellent flowability. Ideal for potting and casting. |
![]() |
EP37-3FLFAOND Highly flexible, low viscosity adhesive. Resistant to severe thermal cycling and thermal shock. Bonds well to dissimilar substrates. Low exotherm system. Long working life. Superior electrical insulation properties. Service temperature range from 4K to +250°F. One to one mix ratio by weight or volume. |
![]() |
EP37-3FLSP Highly flexible. Low viscosity. Optically clear. Serviceable from 4K to +200°F. Superior dimensional stability. Long working life and low exotherm during curing. Ideal for large volume potting and casting. Excellent impact resistant. |
![]() |
EP42HT-2AO-1 Black Good heat conduction. Serviceable from 4K to +400°F. Resists water, oils, fuels. Excellent dielectric properties. Enhanced dimensional stability. Castable up to 2-3 inches thick. Low shrinkage upon cure. Good flow. Meets NASA low outgassing standards. |
![]() |
EP42HT-3AO Thermally conductive, electrically insulative. Ideal for potting and encapsulation. Castable up to 3-4 inches. Excellent chemical resistance. Enhanced thermal cycling capabilities. Good flow. Serviceable from -100°F to +400°F. Impervious to intermittent exposures to steam. Shore D hardnes >80. |
![]() |
EP42HT-4AOMed Black Thermally conductive, electrically insulative two part epoxy. Meets USP Class VI and ISO 10993-5 certifications. Cryogenically serviceable from 4K to +400F. NASA low outgassing aproved. Black in color. For bonding, sealing, coating and casting. |
![]() |
EP50-1.5 Rapid room temperature curing two component epoxy adhesive. Fixturing time of 5-8 minutes. Working life after mixing a 40 gram batch 2-3 minutes. One to one mix ratio by weight or volume. Solid tensile shear strength. Serviceable from 4K to +250°F. Available in different colors and viscosities. |
![]() |
EP51 "5" minute type system. Fast setting. Rapid curing at ambient temperature. Serviceable from 4K to +250°F. Adhesive/sealant. High strength bonds. Good chemical resistance. One to one mix ratio weight or volume. |
![]() |
EP51AN Rapid room temperature curing thermally conductive/electrically insulative adhesive. Fast gelling. Low CTE. Serviceable from 4K to +250°F. High bond strength. Superior heat dissipative properties. Dimensionally stable. Chemical resistant. |
![]() |
EP51AO Rapid curing epoxy adhesive/sealant. Excellent thermal conductivity/electrical insulative properties. Fast set up time. Convenient one to one mix ratio by weight or volume. Serviceable from 4K to +250°F. Resists water, oil, fuels and many solvents. Superior heat dissipation characteristics. |