EP41S-1 Two Part Epoxy EP41S-1

Easily processable, two part epoxy with excellent chemical resistance, particularly to solvents. Available in black. 100% reactive. Low viscosity. Ambient temperature cure. Service temperature range from -60°F to +300°F.

EP41S-1HT Two Part Epoxy System EP41S-1HT

Two component, ambient temperature curing system with excellent physical properties. Thermally stable. High compressive strength. Features extraordinary resistance to fuels, alcohols and organic solvents. Withstands 1,000 hours 85°C/85% RH. Service temperature range -60°F to +400°F. Moderate viscosity. Good electrical insulator.

EP41S-1HTND Two Part Epoxy System EP41S-1HTND

Non-drip two component epoxy resin system. Outstanding chemical resistance to fuels, alcohols, solvents. Smooth paste consistency. Service temperature capability from -60°F to +400°F. High bond strength. Room temperature curing formulation. Low linear shrinkage upon cure.

EP41S-5 Two Part Epoxy System EP41S-5

Excellent chemical resistance to solvents, bases, acids, alcohol and fuels. Withstands exposure to methylene chloride, phenol (10%) and nitric acid (30%). Well suited for coating tanks, pumps and vessels. Moderate viscosity with good flow properties. Can be used for potting/encapsulation. Formidable physical strength properties. Serviceable from -80°F to +450°F.

EP41S-5 Two Part Epoxy System EP41S-5

Excellent chemical resistance to solvents, bases, acids, alcohol and fuels. Withstands exposure to methylene chloride, phenol (10%) and nitric acid (30%). Well suited for coating tanks, pumps and vessels. Moderate viscosity with good flow properties. Can be used for potting/encapsulation. Formidable physical strength properties. Serviceable from -80°F to +450°F.

Low viscosity, chemically resistant epoxy system EP41S-5LV EP41S-5LV

Excellent chemical resistance to solvents, alcohols, fuels, acids and bases. Low viscosity with good flow properties. Can be used for potting/encapsulation. Formidable physical strength properties. Serviceable from -80°F to +350°F.

Two Part Epoxy EP41S-5Med EP41S-5Med

Excellent chemical resistance to solvents, bases, acids, alcohol and fuels. Withstands exposure to methylene chloride, phenol (10%) and nitric acid (30%). Well suited for coating tanks, pumps and vessels. Moderate viscosity with good flow properties. Can be used for potting/encapsulation. Formidable physical strength properties. Serviceable from -80°F to +450°F.

EP41S-5ND Black Two Part Epoxy EP41S-5ND Black

Excellent chemical resistance to solvents, bases, acids, alcohol and fuels. Withstands exposure to methylene chloride, phenol (10%) and nitric acid (30%). Well suited for coating tanks, pumps and vessels. Moderate viscosity with good flow properties. Can be used for potting/encapsulation. Formidable physical strength properties. Serviceable from -80°F to +450°F.

EP41S-6

Excellent chemical resistance to solvents, bases, acids, alcohol and fuels. Withstands exposure to methylene chloride, phenol (10%) and nitric acid (30%). Well suited for coating tanks, pumps and vessels. Moderate viscosity with good flow properties. Can be used for potting/encapsulation. Formidable physical strength properties. Serviceable from -80°F to +450°F.

EP41S-F Two Part Epoxy System EP41S-F

Fast room temperature curing epoxy system. Impressive chemical resistance. Superior electrical insulation properties. 100% reactive. Minimal shrinkage upon cure. Well suited for small sized encapsulating applications. Convenient processing. Service temperature range -60°F to +250°F.