This email was sent to (%email%)
Unsubscribe at: http://www.masterbond.com/phplist/?p=unsubscribe&id=2
Subscribe at: http://www.masterbond.com/phplist/?p=subscribe&id=2
----------------------------------
The following is a news release from Master Bond Inc. You have received it because you are listed as an editor for your publication.
Attached to this email is a low resolution version of the photograph that is included in the press kit for this product.
High resolution versions of this image and files with the body text of this release are available at http://www.masterbond.com/mbnr.html?nr=ep17.
----------------------------------
FOR IMMEDIATE RELEASE
New One Component Adhesive/Sealant
Resists Up To 600°F
HACKENSACK, NJ - May 3, 2006 -- Master Bond Inc., Hackensack, N.J. has developed a new toughened one component heat curing epoxy adhesive/sealant, called EP17. This compound has a service operating range of from -300°F to as high as 600°F. It is formulated to cure at temperatures from 300°F to 350°F for 60-90 minutes. EP17 bonds well to a variety of substrates including metals, glass, ceramics, vulcanized rubbers and many plastics. It has excellent resistance to a wide range of chemicals including fuels, acids, bases, oils and many solvents.
Master Bond EP17 possesses high physical strength properties and is readily machinable. It has superior dimensional stability and very low shrinkage upon cure. Tensile strength is 8,700 psi and tensile modulus is 387,000 psi. EP17 has a Shore D hardness of >90 and a compressive strength of >13,000 psi.
Master Bond EP17 is easy to use. It does not require any mixing prior to use and has an "unlimited" working life at room temperature. It is 100% reactive and does not contain any solvents or diluents. The standard color is gray. Its electrical insulation properties are superior. EP17 is a flowable paste and can also be formulated for application on vertical surfaces without sagging or dripping (EP17ND). The cured adhesive fully meets the requirements of MIL-MMM-A-132 as well as many other specifications.
EP17 is available for use in pint, quart, gallon and 5 gallon containers.
CONTACT:
James Brenner, Marketing Manager
Email: [email protected]
Tel: 201-343-8983
Fax: 201-343-2132
MASTER BOND INC.
154 Hobart Street
Hackensack, NJ 07601-3922
Web: www.masterbond.com
# # #