This email was sent to (%email%)
Unsubscribe at: http://www.masterbond.com/phplist/?p=unsubscribe&id=2
Subscribe at: http://www.masterbond.com/phplist/?p=subscribe&id=2
----------------------------------
The following is a news release from Master Bond Inc. You have received it because you are listed as an editor for your publication.
Attached to this email is a low resolution version of the photograph that is included in the press kit for this product.
High resolution versions of this image and files with the body text of this release are available at http://www.masterbond.com/mbnr.html?nr=ep30flao.
----------------------------------
FOR IMMEDIATE RELEASE
Thermally Conductive,
Low Viscosity Epoxy Features
Cryogenic Serviceability
HACKENSACK, NJ – Aug 12, 2010 – Master Bond EP30FLAO is a two component epoxy resin system for high performance potting, bonding, sealing and coating. It is extremely versatile and can be used in a wide variety of cryogenic applications. This low viscosity epoxy with excellent flow characteristics makes it ideal as a thermally conductive potting compound. It is widely used in the electronic, electrical, computer, metalworking, appliance and chemical industries where electrical insulation, environmental protection and heat transfer is required.
EP30FLAO features a wide service temperature range of 4K to 250ºF. Its thermal conductivity is 9-10 BTU/in/ft²/hr/ºF. The viscosity of the mixed compound is 5,000 to 6,000 cps at 75ºF. In addition to these attractive attributes, it has a low thermal expansion coefficient, superior dimensional stability, good physical strength and toughness.
Parts A and B are available in half pint, pint, quart, one gallon and five gallon containers.
Master Bond’s Cryogenically Serviceable Epoxies
Master Bond’s EP30FLAO is a versatile, two component epoxy system for demanding thermal management applications at cryogenic temperatures. Read more about Master Bond’s cryogenic epoxy formulations at http://www.masterbond.com/lp/tabs/tp_pp_cryogenic.html, or contact Master Bond’s Technical Support Team by phone at +1-201-343-8983, by fax at +1-201-343-2132 or by e-mail at [email protected].
CONTACT:
James Brenner, Marketing Manager
Email: [email protected]
Tel: 201-343-8983
Fax: 201-343-2132
MASTER BOND INC.
154 Hobart Street
Hackensack, NJ 07601-3922
Web: www.masterbond.com
# # #