This email was sent to (%email%)
Unsubscribe at: http://www.masterbond.com/phplist/?p=unsubscribe&id=2
Subscribe at: http://www.masterbond.com/phplist/?p=subscribe&id=2
----------------------------------
The following is a news release from Master Bond Inc. You have received it because you are listed as an editor for your publication.
Attached to this email is a low resolution version of the photograph that is included in the press kit for this product.
High resolution versions of this image and files with the body text of this release are available at http://www.masterbond.com/mbnr.html?nr=ep41smed.
----------------------------------
FOR IMMEDIATE RELEASE
New USP Class VI Approved Epoxy Adhesive
Cures Rapidly at Room Temperature
HACKENSACK, NJ - Jul 30, 2008 -- Master Bond Inc, Hackensack N.J., has introduced a new high performance, low viscosity epoxy adhesive called EP41SMED for fast, room temperature curing, bonding applications. This compound has a 5 to 1 mix ratio by weight and has a “handling” time of as little as 10-15 minutes at ambient temperatures. Bonds are resistant to water, oil, and many organic solvents, as well as cold sterilants, ETO and gamma radiation. It fully meets USP Class VI requirements and conforms to Title 21, US Code of Federal Regulations, FDA Chapter 1, Section 175.105 & 175.300 for food applications.
Master Bond EP41SMED contains no solvents or diluents. It has exceptionally low shrinkage upon cure. Bonds are rigid and offer excellent adhesion to a wide variety of similar and dissimilar substrates. These include metals, glass, ceramics, rubbers, wood and most plastics. Additionally, EP41SMED has superior electrical insulation properties.
EP41SMED is easy to apply and is available for use in pint, quart, gallon and 5 gallon container kits. It has a shelf life in original unopened containers of 6 months minimum.
CONTACT:
James Brenner, Marketing Manager
Email: [email protected]
Tel: 201-343-8983
Fax: 201-343-2132
MASTER BOND INC.
154 Hobart Street
Hackensack, NJ 07601-3922
Web: www.masterbond.com
# # #