This email was sent to (%email%)
Unsubscribe at:  http://www.masterbond.com/phplist/?p=unsubscribe&id=2
Subscribe at: http://www.masterbond.com/phplist/?p=subscribe&id=2

----------------------------------

The following is a news release from Master Bond Inc. You have received it because you are listed as an editor for your publication.

Attached to this email is a low resolution version of the photograph that is included in the press kit for this product.

High resolution versions of this image and files with the body text of this release are available at http://www.masterbond.com/mbnr.html?nr=ep46ht-1.

----------------------------------


FOR IMMEDIATE RELEASE


Epoxy For High Temperature
Service Up To 600°F

HACKENSACK, NJ – Oct 8, 2009 – Developed after years of research, Master Bond EP46HT-1 extends the limits of epoxy adhesive/sealant formulations. It has a continuous service operating temperature range of -100°F to +550°F and can withstand intermittent exposures up to 600°F. EP46HT-1 has a glass transition temperature of over 235°C. In addition to high temperatures, it is also designed to withstand severe and repeated thermal cycling.

Master Bond EP46HT-1 is easy to apply and cures rapidly at elevated temperatures. It is 100% reactive and does not contain any solvents or diluents. It offers exceptional physical strength, outstanding dimensional stability, and superior chemical resistance. EP46HT-1 has excellent adhesion to metals, glass, vulcanized rubbers, and most plastics. The hardened system is an electrical insulator. Applications range from downhole oil drilling to turbo compressors and satellite modules.

 

CONTACT:
James Brenner, Marketing Manager
Email: [email protected]
Tel: 201-343-8983
Fax: 201-343-2132

MASTER BOND INC.
154 Hobart Street
Hackensack, NJ 07601-3922
Web: www.masterbond.com

# # #