This email was sent to (%email%)
Unsubscribe at:  http://www.masterbond.com/phplist/?p=unsubscribe&id=2
Subscribe at: http://www.masterbond.com/phplist/?p=subscribe&id=2

----------------------------------

The following is a news release from Master Bond Inc. You have received it because you are listed as an editor for your publication.

Attached to this email is a low resolution version of the photograph that is included in the press kit for this product.

High resolution versions of this image and files with the body text of this release are available at http://www.masterbond.com/mbnr.html?nr=ep62-1med.

----------------------------------


FOR IMMEDIATE RELEASE


New USP Class VI Approved Epoxy
Adhesive Resists Sterilants

HACKENSACK, NJ - Aug 4, 2006 -- Master Bond Inc, Hackensack, N.J. has developed EP62-1MED, a new, two component epoxy adhesive system which features outstanding chemical and temperature resistance. This compound is specifically designed to withstand repeated cycles of steam, ethylene oxide, radiation and chemical sterilization. EP62-1MED cures at moderately elevated temperatures (150°F-200°F) and offers an exceptional long working life at room temperatures. It contains no solvents or volatiles and has a 100 to 10 mix ratio by weight.

EP62-1MED has excellent bond strength to metals, glass, ceramics, wood and most plastics. It has outstanding durability and is serviceable up to 400°F. Shrinkage upon cure is exceptionally low (<0.06%). The color of part A is clear and part B is brown. EP62-1MED is available in pint, quart, gallon and 5 gallon kits. It is also available in convenient gun applicators for ease of use.

 

CONTACT:
James Brenner, Marketing Manager
Email: [email protected]
Tel: 201-343-8983
Fax: 201-343-2132

MASTER BOND INC.
154 Hobart Street
Hackensack, NJ 07601-3922
Web: www.masterbond.com

# # #