FOR IMMEDIATE RELEASE

Master Bond Inc. Introduces UV19,
A New Flexible, Low Viscosity UV Curable
Compound Specially Designed For High Performance
Laminating, Sealing, Bonding And Coating

HACKENSACK, NJ - Apr 18, 2005 -- Master Bond Inc. of Hackensack, New Jersey has developed UV19, a new low viscosity, flexible UV curable composition formulated for fast, high performance laminating, sealing, bonding and casting. It is an optically clear, mobile liquid which cures readily upon exposure to UV light at ambient temperatures to a flexible strong solid with superior mechanical strength properties and excellent adhesion to many different substrates including most plastics and glasses as well as metals. The UV19 system is 100% reactive and does not contain any volatiles. Unlike many other commercially offered UV curing compounds, its cure is not inhibited by air and it exhibits minimal shrinkage when cured. UV19 has excellent resistance to water and many other aggressive chemicals.

Master Bond UV19’s low viscosity of less than 300cps at 75°F enhances its utility for laminating as well as sealing, bonding and coating applications. Its excellent flexibility (over 100% elongation) and outstanding adhesive properties make it particularly attractive for laminating, sealing and bonding to substrates with widely different thermal expansion coefficients such as, for example, glass and polycarbonate. UV19 has a tensile strength in excess of 800 psi and remarkably high impact strength, abrasion resistance and heat stability. This unique combination of processing and performance characteristics has resulted in broad acceptance for many volume industrial applications where currently available products cannot meet the diverse properties exhibited by the Master Bond UV19 system.

CONTACT:
James Brenner, Marketing Manager
Email: [email protected]
Tel: 201-343-8983
Fax: 201-343-2132

MASTER BOND INC.
154 Hobart Street
Hackensack, NJ 07601-3922
Web: www.masterbond.com

# # #