This email was sent to (%email%)
Unsubscribe at:  http://www.masterbond.com/phplist/?p=unsubscribe&id=2
Subscribe at: http://www.masterbond.com/phplist/?p=subscribe&id=2

----------------------------------

The following is a news release from Master Bond Inc. You have received it because you are listed as an editor for your publication.

Attached to this email is a low resolution version of the photograph that is included in the press kit for this product.

High resolution versions of this image and files with the body text of this release are available at http://www.masterbond.com/mbnr.html?nr=uv22.

----------------------------------


FOR IMMEDIATE RELEASE


UV Curable Nanosilica Filled Epoxy
Has Outstanding Physical Strength and
Exceptional Abrasion & Chemical Resistance

HACKENSACK, NJ – Jun 16, 2009 – Master Bond Inc. of Hackensack, NJ is proud to announce an incredible breakthrough in polymer technology. Master Bond UV22 is a nanosilica reinforced, UV curable epoxy system that offers a combination of properties not available in conventional epoxy systems. The nano-sized filler (<50nm) gives the cured system exceptional abrasion resistance, excellent optical clarity, low shrinkage and superb physical strength properties, while still allowing the product to have an advantageously low viscosity of 4,000 cps. The tensile strength of the cured epoxy is greater than 4,600 psi and its tensile modulus is greater than 500,000 psi. This represents an amazing 50-90% improvement in performance over similar unreinforced systems.

Master Bond UV22 cures rapidly upon exposure to UV light at room temperatures. It is a single component system and requires no mixing. It has a low coefficient of thermal expansion and is a superior electrical insulator. Post curing UV22 enhances its temperature and chemical resistance properties. For example, post curing at 90-125°C for 30 minutes will give it a glass transition temperature of greater than 120°C, far higher than traditional UV cure systems. Its ability to withstand exposure to solvents, acids and bases is also greatly improved. UV22 has a service temperature range of -60 to +300°F.

Master Bond UV22 is easy to apply and is available for use in convenient syringe applicators. Environmentally friendly, UV22 is solvent-free and not oxygen inhibited. UV22 is also available in a specially formulated, dual-cure version called UV22DC, which can be cured by UV light or by the application of heat, making it an excellent solution for applications which feature “shadowed out” areas not reachable by UV light.

 

CONTACT:
James Brenner, Marketing Manager
Email: [email protected]
Tel: 201-343-8983
Fax: 201-343-2132

MASTER BOND INC.
154 Hobart Street
Hackensack, NJ 07601-3922
Web: www.masterbond.com

# # #