Designed for medical device manufacturing, MasterSil 711Med passes ISO 10993-5 testing. It is a one part, flowable, room temperature vulcanizing (RTV) silicone which needs no mixing, and can be used for bonding, sealing, coating and form-in-place gasketing applications. This non-corrosive, translucent compound withstands many sterilization methods, including liquid sterilants, gamma radiation and EtO.
MasterSil 711Med cures very quickly upon exposure to humidity or moisture. Curing speed is influenced by the humidity level, with higher humidity in the applied areas resulting in a faster cure. Additionally, thinner sections cure more quickly than thicker ones. Tack-free time at 75°F and over 50% humidity is 2-5 minutes. Once cured, it delivers high temperature resistance up to 400°F. This compound is electrically insulative, with a volume resistivity greater than 1014 ohm-cm at room temperature. Featuring superior flexibility, it is able to withstand thermal cycling, vibration and shock, with an elongation measuring between 300-400%. Its Shore A hardness is 25-35.
MasterSil 711Med bonds well to a variety of substrates including metals, glass, ceramics, many plastics and cured silicone rubber. It is packaged in 30 cc syringes, which are equally convenient for automated and manual dispensing.
Master Bond MasterSil 711Med is a one component, medical grade silicone adhesive that resists temperatures up to 400°F. Read more about Master Bond’s one part, no mix, tin catalyzed RTV silicones at https://www.masterbond.com/products/one-part-silicone-adhesives-sealants-and-coatings or contact Tech Support. Phone: +1-201-343-8983 Fax: +1-201-343-2132 Email: technical@masterbond.com.
Note to Editors:
For a full product description, please visit: https://www.masterbond.com/tds/mastersil-711med
  Check out new videos on our YouTube channel: https://www.youtube.com/user/MasterBondVideo
 
You can embed any of our videos on your website.
CONTACT
  James Brenner, Marketing Manager
  Email: jbrenner@masterbond.com
  Tel: +1-201-343-8983
  Fax: +1-201-343-2132
MASTER BOND INC.
  154    Hobart Street 
  Hackensack,   NJ 07601-3922 
  Web: www.masterbond.com
# # #