EP38
Two component epoxy for potting, bonding, sealing and coating
Key Features
- High optical clarity
- Electrically insulative
- High strength properties
- Outstanding chemical resistance
- Fast cures at room or elevated temperatures
- Protects against boiling water
Typical Properties
Viscosity
Part A: 11,000-15,000 cps, Part B: 2,500-3,800 cps
Cure Schedule
75°F: 24-48 hours; 200°F: 1-2 hours
Hardness
>80 Shore D
Service Temperature Range
-60°F to +250°F
Tensile Modulus
>350,000 psi
Volume Resistivity
>10¹⁴ ohm-cm