EP30-4
Optically clear, two component epoxy for bonding, coating, sealing and casting
Key Features
- Low viscosity
- Fast curing, even in thin sections
- Low shrinkage upon cure
- Highly desirable for potting and encapsulating
Typical Properties
Viscosity
Part A: 1,000-3,000 cps, Part B: 20-100 cps
Cure Schedule
Cure schedule at 75°F: 24 hours.
Hardness
75-85 Shore D
Service Temperature Range
-60°F to +250°F
Dielectric Constant
4.3
Refractive Index
1.55