EP30P
Low viscosity, two component epoxy system with excellent performance and compatibility with polycarbonates, acrylics and glass
Key Features
- Outstanding optical clarity
- Superb strength profile
- Meets FDA Chapter 1, Section 175.105 for indirect food applications
- Can be utilized for bonding, sealing, coating and encapsulation
Typical Properties
Viscosity
1,200-1,400 cps
Cure Schedule
75°F: 24-48 hours; 200°F: 2-3 hours
Hardness
>75 Shore D
Service Temperature Range
-60°F to +250°F
Dielectric Constant
3.6
Refractive Index
1.56