UV16

Low viscosity, one component, UV curable epoxy based system
Key Features
  • Good physical strength properties
  • Low shrinkage upon curing
  • Cationic curing system, no oxygen inhibition
  • Passes NASA low outgassing tests
Typical Properties
Viscosity
250-500 cps
Cure Schedule
UV light 320-365 nm for 15-30 seconds
Hardness
70-80 Shore D
Service Temperature Range
-80°F to +400°F
Glass Transition Temperature (Tg)
95-100°C
Refractive Index
1.511
Bild
UV16 One Part UV Curable Compound
Certifications

Meets EU Directive 2015/863

ASTM E595 Compliant

Product Description

Master Bond UV16 is a low viscosity, high strength epoxy based UV curable system for bonding, sealing and coating. It is 100% reactive and does not contain any solvents or other volatiles. It also exhibits no oxygen inhibition. UV16 will cure quickly and easily when exposed to a UV light source with a wavelength range between 320-365 nm, with the optimum at 365 nm. The energy required is typically 20-40 milliwatts per cm². UV16 is highly reactive and will cure exceptionally fast when exposed to UV light. The rate of cure depends upon the distance of the light from the material being cured, the thickness of the section and the intensity of the light source. It typically cures in thicknesses of 0.001-0.002 inches up to 0.120 inches. Thinner sections will cure in a few seconds while thicker sections will normally cure in 30-60 seconds. UV16 has excellent resistance to a wide variety of chemicals including water, acids, bases, fuels and many solvents. It has superb physical strength characteristics and electrical insulation properties. UV16 has superior adhesion to a wide variety of substrates including plastics, glass and many metals. UV16 has stellar optical clarity and light transmission properties.

Cationic systems, such as UV16, tend to have much higher temperature resistance than other UV type systems. The glass transition temperature (Tg) with a straight UV cure is 95-100°C and when post cured for 30 minutes at 125°C, the Tg is 135-140°C. This post cure also enhances its chemical resistance. The service temperature range is -80°F to +400°F. It is widely used for a variety of applications in the optical, optoelectronic, aerospace and related industries.

Product Advantages

  • One component system; no mixing needed
  • Very low viscosity, easily applied
  • Cationic curing system, no oxygen inhibition
  • Superior temperature resistance
  • Outstanding optical clarity
  • High bond strength; excellent adhesion to surface treated metals, glass and many plastics
  • Excellent dimensional stability
Show More

How to order

Verify Your Product Selection

With thousands of custom formulations available, our expert engineers provide personalized consultation to ensure you select the ideal adhesive. We will follow up with a product and packaging recommendation for your specific application.

Get a Quote

Our customer service team will follow up with a detailed quote with packaging and shipping options.

Place Your Order

We'll work with your company to process the order efficiently.

Receive Your Material

Your adhesive will be made to order and shipped to you. Typical lead times are 10-14 business days, with rush options available for urgent orders.