UV16
Low viscosity, one component, UV curable epoxy based system
Key Features
- Good physical strength properties
- Low shrinkage upon curing
- Cationic curing system, no oxygen inhibition
- Passes NASA low outgassing tests
Typical Properties
Viscosity
250-500 cps
Cure Schedule
UV light 320-365 nm for 15-30 seconds
Hardness
70-80 Shore D
Service Temperature Range
-80°F to +400°F
Glass Transition Temperature (Tg)
95-100°C
Refractive Index
1.511
Bild
Discuss with a Specialist
(1-2 Business Day Request) Get Technical Data sheet
(Instant Email Delivery) Request Safety Data sheet
(1-2 Business Day Request)
(1-2 Business Day Request) Get Technical Data sheet
(Instant Email Delivery) Request Safety Data sheet
(1-2 Business Day Request)
Applications
Certifications
Meets EU Directive 2015/863
ASTM E595 Compliant
Case Study
UV16: Utilized in Bonding Applications for Microring Resonators, Optical Waveguides and Confocal Microscopes
In several published research articles, patents, and manufacturers’ specifications, scientists and engineers have identified UV16 for use in their applications due to its unparalleled performance in one or more areas. The table below highlights two r …