LED401LV

One component LED curable system for high performance bonding, sealing, coating and encapsulation
Key Features
  • Cures with LED light source, no UV light required
  • Cures tack-free without oxygen inhibition
  • Excellent physical strength properties
  • Withstands 1,000 hours 85°C/85% RH
Typical Properties
Viscosity
60,000-80,000 cps
Cure Schedule
Cure with LED at 405 nm at ~ 1-4 watts/cm² intensity for 15-30 seconds or longer in thicker sections.
Hardness
65-75 Shore D
Service Temperature Range
-60°F to +250°F
Coefficient of Thermal Expansion
60-65 X 10⁻⁶ in/in/°C
Volume Resistivity
>10¹⁴ ohm-cm
Bild
LED401LV One Part LED Curing System
Certifications

Meets EU Directive 2015/863

1,000 Hours at 85°C/85% RH

Product Description

Master Bond LED401LV is a highly innovative, one part LED type system that cures fully upon exposure to a 405 nm wavelength light source where the presence of any UV light is minimal or incidental. In fact, this unique system will fully cure tack-free without any oxygen inhibition. This breakthrough technology allows LED401LV to be utilized not only as an adhesive, but as a sealant, coating and encapsulation material. This remarkable system can cure in sections up to and beyond 1/8 inch thick upon exposure to the LED light. Since it is a LED curable system, it is intrinsically safer than one requiring UV light for polymerization, as LED light emitting sources are generally considered to be less hazardous and more user friendly than their comparable UV counterparts. Master Bond LED401LV requires no mixing and will cure rapidly, with the speed of cure dependent upon the intensity of the light source, the thickness of the layer and the distance of the light source from the material being cured. Realistically, the light intensity should be 1-4 watts/cm2. Master Bond strongly advises end users to consult with their light source provider to ascertain the best LED for their particular application, along with details on the wavelength being emitted by the light source. In thinner sections, full cures can be achieved in 15-30 seconds (sometimes less than that), while thicker sections require longer cure times. It also bonds well to glass, polycarbonates and acrylics, along with other plastics and metals. It has excellent optical clarity and light transmission properties, with a very slight amber tint. Additionally, the formulation is solvent-free. Other versions of this product are available with different viscosities and with an opaque white color.

Product Advantages

  • Outstanding optical clarity; excellent light transmission
  • Very good dimensional stability
  • High bond strength with superior adhesion to surface treated metals, glass and many plastics
  • Superb electrical insulation properties
  • High viscosity yet maintains flowability
  • Very good chemical resistance to water, many acids, bases and oils
Show More

How to order

Verify Your Product Selection

With thousands of custom formulations available, our expert engineers provide personalized consultation to ensure you select the ideal adhesive. We will follow up with a product and packaging recommendation for your specific application.

Get a Quote

Our customer service team will follow up with a detailed quote with packaging and shipping options.

Place Your Order

We'll work with your company to process the order efficiently.

Receive Your Material

Your adhesive will be made to order and shipped to you. Typical lead times are 10-14 business days, with rush options available for urgent orders.