EP41S-5LV
Two component epoxy system featuring excellent chemical resistance especially to solvents, acids, bases, alcohols and fuels
Key Features
- Convenient handling
- Low exotherm
- Superior electrical insulation properties
- Withstands aggressive chemicals including methylene chloride
Typical Properties
Viscosity
2,000-5,000 cps
Cure Schedule
75°F: 3-5 days; 150-200°F: 2-3 hours
Hardness
85-95 Shore D
Service Temperature Range
-80°F to +350°F
Glass Transition Temperature (Tg)
120-125°C
Volume Resistivity
>10¹⁴ ohm-cm
Bild
Discuss with a Specialist
(1-2 Business Day Request) Get Technical Data sheet
(Instant Email Delivery) Request Safety Data sheet
(1-2 Business Day Request)
(1-2 Business Day Request) Get Technical Data sheet
(Instant Email Delivery) Request Safety Data sheet
(1-2 Business Day Request)
Applications
Certifications
ASTM E595 Compliant
Meets EU Directive 2015/863
Packaging