UV15X-6Med-2LV
UV system for high performance bonding, sealing and coating
Key Features
- Superior abrasion resistance
- Meets ISO 10993-5
- High flexibility and toughness
- Moderate viscosity
Typical Properties
Viscosity
20,000-40,000 cps
Cure Schedule
10-30 seconds when exposed to a UV light source emitting at a wavelength of 320-365 nm with an energy output as low as 20-40 milliwatts/cm2
Hardness
55-65 Shore D
Service Temperature Range
-80°F to +250°F
Elongation
>100%
Refractive Index
1.50