UV15X-6Med-2LV

UV system for high performance bonding, sealing and coating
Key Features
  • Superior abrasion resistance
  • Meets ISO 10993-5
  • High flexibility and toughness
  • Moderate viscosity
Typical Properties
Viscosity
20,000-40,000 cps
Cure Schedule
10-30 seconds when exposed to a UV light source emitting at a wavelength of 320-365 nm with an energy output as low as 20-40 milliwatts/cm2
Hardness
55-65 Shore D
Service Temperature Range
-80°F to +250°F
Elongation
>100%
Refractive Index
1.50
Image
UV15X-6Med-2LV One Part UV Curable System
Certifications

Meets EU Directive 2015/863

ISO 10993-5 for Cytotoxicity

Product Description

Master Bond UV15X-6Med-2LV is a one component, medium viscosity UV system featuring high flexibility, excellent toughness and superior abrasion resistance. It can be used for a wide variety of applications including bonding, sealing, coating and encapsulation. Its robust flexibility allows it to withstand severe thermal cycling as well as resisting thermal and mechanical shocks. UV15X-6Med-2LV bonds well to a variety of substrates, especially glass, polycarbonates and acrylics as well as many other plastics, metals and rubbers. It has good chemical resistance to water, cleaning agents, chemical sterilants, EtO and gamma radiation. UV15X-6Med-2LV is a top notch thermal and electrical insulator with a service temperature range of -80°F to +250°F.

UV15X-6Med-2LV generally cures readily in 20-30 seconds when exposed to a UV light source emitting at a wavelength of 320-365 nm with an energy output as low as 20-40 milliwatts/cm². The rate of cure depends upon the system’s distance from the light source, the thickness of the section and of course the intensity of the light source. It should be noted that the system can cure in sections approaching 1/4 inch thick. However, when bonding, sections of a few thousandths of an inch are more than adequate. Most importantly, UV15X-6Med-2LV does not display oxygen inhibition. This system is widely used in medical device manufacturing and specialty applications where ISO 10993-5 requirements are desirable.

Product Advantages

  • One part system with no mixing needed
  • Cures fast upon exposure to 320-365 nm UV light at ambient temperatures. No oxygen inhibition
  • Outstanding toughness and abrasion resistance
  • Withstands rigorous thermal cycling
  • Passes ISO 10993-5 for cytotoxicity
Show More

How to order

Verify Your Product Selection

With thousands of custom formulations available, our expert engineers provide personalized consultation to ensure you select the ideal adhesive. We will follow up with a product and packaging recommendation for your specific application.

Get a Quote

Our customer service team will follow up with a detailed quote with packaging and shipping options.

Place Your Order

We'll work with your company to process the order efficiently.

Receive Your Material

Your adhesive will be made to order and shipped to you. Typical lead times are 10-14 business days, with rush options available for urgent orders.