EP42HT-2ANLV
Two part, room temperature curable epoxy adhesive, sealant, coating and casting system
Key Features
- Convenient handling, long working life
- High thermal conductivity and electrical insulation
- Superior chemical resistance
- Good flow properties
Typical Properties
Viscosity
Part A: 80,000-120,000 cps, Part B: 4,000-10,000 cps
Cure Schedule
overnight at 75°F, followed by 2-3 hours at 150-200°F
Hardness
85-95 Shore D
Service Temperature Range
-100°F to +350°F
Coefficient of Thermal Expansion
22-27 X 10⁻⁶ in/in/°C
Tensile Strength
4,500-5,500 psi