EP42HT-2ANLV

Two part, room temperature curable epoxy adhesive, sealant, coating and casting system
Key Features
  • Convenient handling, long working life
  • High thermal conductivity and electrical insulation
  • Superior chemical resistance
  • Good flow properties
Typical Properties
Viscosity
Part A: 80,000-120,000 cps, Part B: 4,000-10,000 cps
Cure Schedule
overnight at 75°F, followed by 2-3 hours at 150-200°F
Hardness
85-95 Shore D
Service Temperature Range
-100°F to +350°F
Coefficient of Thermal Expansion
22-27 X 10⁻⁶ in/in/°C
Tensile Strength
4,500-5,500 psi
Immagine
EP42HT-2ANLV Two Component Epoxy
Certifications

Meets EU Directive 2015/863

Packaging
Product Description

Master Bond EP42HT-2ANLV is a two component epoxy adhesive, sealant, coating and casting system featuring thermal conductivity and electrical insulation. It has a forgiving mix ratio of 100 to 40 by weight and flows well. It cures readily at ambient temperatures or more rapidly with heat. The optimum cure schedule is overnight at room temperature, followed by 2-3 hours at 150-200°F. Since it is a filled system, it has exceptionally low shrinkage and stellar dimensional stability.

EP42HT-2ANLV bonds well to a wide variety of substrates, including metals, composites, glass, ceramics, rubbers and plastics. It generates very little heat when curing and can be used for potting and casting up to 3-4 inches thick. The system has excellent chemical resistance to water, oils, fuels, acids and bases. Its temperature range is -100°F to +350°F. The color of Part A is off white and Part B is amber. EP42HT-2ANLV is a viable candidate in aerospace, electronic, optical, and specialty OEM where good flow and thermal conductivity combined with electrical insulation are essential to the application.

Product Advantages

  • Long working life
  • Good flow properties
  • Superior heat conduction
  • Excellent temperature resistance
  • Noteworthy physical property profile
Show More

How to order

Verify Your Product Selection

With thousands of custom formulations available, our expert engineers provide personalized consultation to ensure you select the ideal adhesive. We will follow up with a product and packaging recommendation for your specific application.

Get a Quote

Our customer service team will follow up with a detailed quote with packaging and shipping options.

Place Your Order

We'll work with your company to process the order efficiently.

Receive Your Material

Your adhesive will be made to order and shipped to you. Typical lead times are 10-14 business days, with rush options available for urgent orders.