EP4CL-80Med

One component, optically clear epoxy for bonding and sealing that cures at 80°C to 85°C for medical applications
Key Features
  • Ultra low viscosity
  • Not premixed and frozen
  • High glass transition temperature
  • Meets ISO 10993-5
Typical Properties
Viscosity
50-150 cps
Cure Schedule
60-90 minutes at 80-85°C or 10-15 minutes at 100°C
Hardness
85-95 Shore D
Service Temperature Range
-80°F to +450°F
Glass Transition Temperature (Tg)
155-160°C
Refractive Index
1.52
Bild
One Part Epoxy EP4CL-80Med
Certifications

ISO 10993-5 for Cytotoxicity

Meets EU Directive 2015/863

Product Description

Master Bond EP4CL-80Med is a one part, optically clear, very low viscosity epoxy for bonding, sealing and coating. It will cure easily at 80°C to 85°C in 60-90 minutes or at 100°C in 10-15 minutes. Since it is not premixed and frozen, it is a true one part system, and has an unlimited working life at room temperature. It should be stored in the refrigerator. EP4CL-80Med possesses excellent dimensional stability and low shrinkage upon curing.

EP4CL-80Med bonds well to a several substrates such as metals, composites, ceramics and many plastics. It has exceptionally robust physical strength properties, especially, tensile strength and modulus. It has superb light transmission from 360 nm to 1500 nm. Its low viscosity allows it to be applied by brushing, spraying, and in some situations, can be spin coated onto a substrate.

EP4CL-80Med has good resistance to a wide variety of sterilization methods, including autoclaving, dry heat, radiation, chemical sterilants and most notably, vaporized hydrogen peroxide. This epoxy is a reliable electrical and thermal insulator, and its service temperature range is -62°C to +232°C (-80°F to +450°F). EP4CL-80Med can be considered in a large array of medical applications including endoscope production and repair, surgical devices, or virtually any medical instrumentation where an optically clear, medical grade epoxy is required.

Product Advantages

  • Single component, no mixing needed
  • Cures at 80-85°C
  • Convenient packaging
  • Can withstand repeated sterilization
  • Transparent
  • Meets ISO 10993-5
Show More

How to order

Verify Your Product Selection

With thousands of custom formulations available, our expert engineers provide personalized consultation to ensure you select the ideal adhesive. We will follow up with a product and packaging recommendation for your specific application.

Get a Quote

Our customer service team will follow up with a detailed quote with packaging and shipping options.

Place Your Order

We'll work with your company to process the order efficiently.

Receive Your Material

Your adhesive will be made to order and shipped to you. Typical lead times are 10-14 business days, with rush options available for urgent orders.