EP3HTSCN One Part Epoxy
EP3HTSCN
One part, high performance, electrically conductive epoxy
Tensile Lap Shear Strength
900-1,100 psi
Volume Resistivity
0.05 to 0.10 ohm-cm
  • RoHS Compliant
  • Coating
  • Bonding
  • Sealing
  • Gap Filling
paste cures readily at 250°F at 45-50 minutes or in just 20-30 minutes at 300°F 75-85 Shore D -60°F to +400°F /de/tds/ep3htscn
EP3HTSDA-2Med One Part Silver Filled Epoxy
EP3HTSDA-2Med
One component, medical grade, electrically conductive epoxy featuring exceptionally high thermal conductivity
Thermal Conductivity
45-49 BTU•in/(ft²•hr•°F) W/(m•K)]
Volume Resistivity
<0.001 ohm-cm
  • ISO 10993-5 for Cytotoxicity
  • RoHS Compliant
  • Bonding
  • Die Attach
  • Gap Filling
  • Sealing
  • Coating
>400,000 cps 250°F for 20-30 minutes, 300°F for 5-10 minutes 75-85 Shore D -80°F to +450°F /de/tds/ep3htsda-2med
EP3HTSMed One Part Medical Grade Epoxy
EP3HTSMed
One part, electrically conductive, biocompatible epoxy system
Tensile Lap Shear Strength
>400 psi
Volume Resistivity
<0.001 ohm-cm
  • USP Class VI Medical
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Gap Filling
paste 40-90 minutes at 250°F or 20-40 minutes at 300°F (minimum cure temperature is 235-240°F) 60-80 Shore D -60°F to +400°F /de/tds/ep3htsmed
EP3RR-80: One Part Epoxy System
EP3RR-80
One component epoxy system for bonding, sealing, potting and encapsulation applications featuring curing temperatures of 175-180°F or higher
Dielectric Constant
4.4
Volume Resistivity
10¹⁴ ohm-cm
  • MIL-STD-810G for Fungus Resistance
  • NASA Low Outgassing
  • 1,000 Hours at 85°C/85% RH
  • RoHS Compliant
  • Sealing
  • Encapsulation
  • Potting
  • Bonding
60,000-120,000 cps Cure in 45-50 minutes at 175-180°F, or in 25-30 minutes 250°F 80-90 Shore D -100°F to +350°F /tds/ep3rr-80
EP3SP5FL-ND2 One Part Snap Cure Epoxy
EP3SP5FL-ND2
One component “snap cure” epoxy adhesive with paste viscosity
Elongation
10-15%
Tensile Lap Shear Strength
>2,000 psi
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Gap Filling
paste 1-2 minutes at 300°F >85 Shore D -60°F to +200°F /tds/ep3sp5fl-nd2
EP3UF One Part Epoxy Adhesive System
EP3UF
One component epoxy for bonding and underfill applications
Dielectric Strength
450 volts/mil
Volume Resistivity
>10¹² ohm-cm
  • NASA Low Outgassing
  • RoHS Compliant
  • Bonding
  • Underfill
  • Sealing
  • Coating
  • Encapsulation
10,000-40,000 cps 20-30 minutes at 250°F or 10-15 minutes at 300°F 80-90 Shore D -60°F to +300°F /de/tds/ep3uf
EP3UF-1 One Component Epoxy
EP3UF-1
One component epoxy for bonding and underfill applications
Dielectric Strength
450 volts/mil
Volume Resistivity
>10¹² ohm-cm
  • RoHS Compliant
  • Bonding
  • Underfill
  • Sealing
  • Coating
  • Encapsulation
5,000-15,000 cps 20-30 minutes at 250°F or 10-15 minutes at 300°F 80-90 Shore D -60°F to +250°F /de/tds/ep3uf-1
EP4CL-80
One component, optically clear epoxy for bonding and sealing that cures at 80°C to 85°C
Glass Transition Temperature (Tg)
155-160°C
Refractive Index
1.52
  • RoHS Compliant
  • NASA Low Outgassing
  • Bonding
  • Sealing
  • Coating
  • Underfill
50-150 cps 60-90 minutes at 80-85°C or 10-15 minutes at 100°C 85-95 Shore D -80°F to +450°F /de/tds/ep4cl-80
One Part Epoxy EP4CL-80Med
EP4CL-80Med
One component, optically clear epoxy for bonding and sealing that cures at 80°C to 85°C for medical applications
Glass Transition Temperature (Tg)
155-160°C
Refractive Index
1.52
  • ISO 10993-5 for Cytotoxicity
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Impregnation
  • Underfill
50-150 cps 60-90 minutes at 80-85°C or 10-15 minutes at 100°C 85-95 Shore D -80°F to +450°F /de/tds/ep4cl-80med
EP4G-80
One component, graphite filled epoxy with a curing temperature of 80°C
Glass Transition Temperature (Tg)
130-140°C
Volume Resistivity
50-100 ohm-cm
  • NASA Low Outgassing
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Gap Filling
4,000-10,000 cps 60-90 minutes at 80°C 75-85 Shore D -58°F to +347°F /de/tds/ep4g-80