Product Selector

Filters
Applications
Product Type
Certifications
Thermal Conductivity
Product Certifications Applications Viscosity Cure Schedule Hardness Temp. Range Link to Content
EP42HT-2LO Two Part Epoxy System
EP42HT-2LO
Two component epoxy adhesive, sealant, coating and casting system
Dielectric Constant
3.8
Volume Resistivity
>10¹⁴ ohm-cm
  • NASA Low Outgassing
  • 1,000 Hours at 85°C/85% RH
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Casting
  • Encapsulation
  • Gap Filling
Part A: 55,000-110,000 cps, Part B: 30 - 70 cps 75°F for 48-72 hours, 200°F for 2-3 hours 80-90 Shore D -60°F to +450°F /de/tds/ep42ht-2lo
EP42HT-2Med Two Part Epoxy
EP42HT-2Med

Two component, high temperature resistant epoxy for medical device assembly; tested and approved for 3 medical related certifications

Acoustical Impedance
3.1 MRayl
Glass Transition Temperature (Tg)
150-155°C
  • ISO 10993-5 for Cytotoxicity
  • USP Class VI Medical
  • RoHS Compliant
  • ISO 10993-10 for Skin Sensitization
  • Bonding
  • Sealing
  • Coating
  • Potting
  • Encapsulation
  • Gap Filling
  • Casting
Part A: 55,000-110,000 cps, Part B: 30 - 70 CPS overnight at 75°F followed by 2-4 hours at 150-250°F 75-85 Shore D -60°F to 450°F /de/tds/ep42ht-2med
EP4EN-80 One Component Epoxy
EP4EN-80
One component flowable epoxy for bonding and small encapsulation applications with a curing schedule at 80°C to 85°C
Dielectric Constant
4.4
Thermal Conductivity
5.2-5.9 BTU•in/(ft²•hr•°F) [0.75-0.85 W/(m•K)]
  • NASA Low Outgassing
  • RoHS Compliant
  • Bonding
  • Encapsulation
  • Potting
600-1,800 cps 90 minutes at 65°C plus 30 minutes at 80-85°C 85-95 Shore D -58°F to +302°F /de/tds/ep4en-80
EP5G-80 One Component Epoxy
EP5G-80
One component, graphite filled epoxy with a curing temperature of 80°C
Glass Transition Temperature (Tg)
130-140°C
Volume Resistivity
5-15 ohm-cm
  • NASA Low Outgassing
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
30,000-300,000 cps 4 hours at 80°C 75-85 Shore D -58°F to +347°F /de/tds/ep5g-80
EP5TC-80 One Component Paste Epoxy
EP5TC-80
One component thermally conductive, electrically insulating epoxy with a curing temperature of 80°C
Dielectric Constant
4.6
Volume Resistivity
>10¹² ohm-cm
  • NASA Low Outgassing
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
60,000-180,000 cps 80°C for 90-120 minutes with an optional post cure of 1-2 hours at 80°C to optimize properties 90-100 Shore D -58°F to +302°F /de/tds/ep5tc-80
Two Component Epoxy EP62-1ND
EP62-1ND
Two component epoxy resin system featuring excellent temperature and chemical resistance, non-drip application
Tensile Lap Shear Strength
8,000-9,000 psi
Volume Resistivity
>10¹⁴ ohm-cm
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Gap Filling
paste 4-6 hours at 140-158°F [60-70°C], 20-40 minutes at 176-212°F [80-100°C] or 10-20 minutes at 257°F [125°C] 75-85 Shore D -60°F to +450°F /de/tds/ep62-1nd
EP65HT-1 Two Part Epoxy
EP65HT-1
Two component epoxy system featuring the special combination of very fast setup times and high temperature resistance
Dielectric Constant
4.1
Glass Transition Temperature (Tg)
125-130°C
  • NASA Low Outgassing
  • RoHS Compliant
  • 1,000 Hours at 85°C/85% RH
  • Bonding
  • Sealing
  • Coating
  • Gap Filling
Part A: 55,000-110,000 cps, Part B: 8,000-12,000 cps 3-5 minutes setup, full cure within 6-12 hours at 75°F 80-90 Shore D -60°F to +400°F /de/tds/ep65ht-1
LED401LV One Part LED Curing System
LED401LV
One component LED curable system for high performance bonding, sealing, coating and encapsulation
Coefficient of Thermal Expansion
60-65 X 10⁻⁶ in/in/°C
Volume Resistivity
>10¹⁴ ohm-cm
  • RoHS Compliant
  • 1,000 Hours at 85°C/85% RH
  • Bonding
  • Sealing
  • Coating
  • Encapsulation
60,000-80,000 cps Cure with LED at 405 nm at ~ 1-4 watts/cm² intensity for 15-30 seconds or longer in thicker sections. 65-75 Shore D -60°F to +250°F /de/tds/led401lv
LED405Med
One component, nanosilica filled LED curable system
Coefficient of Thermal Expansion
35-40 X 10⁻⁶ in/in/°C
Dielectric Constant
4.2
  • ISO 10993-5 for Cytotoxicity
  • RoHS Compliant
  • Bonding
  • Coating
  • Sealing
  • Encapsulation
2,000-8,000 cps Cure with LED at 405 nm at ~ 1-4 watts/cm² intensity for 15-30 seconds or longer in thicker sections. 65-75 Shore D -60°F to +250°F /de/tds/led405med
One Part Adhesive LED415DC90
LED415DC90
One component, flexibilized LED curable system
Tensile Modulus
450,000-550,000 psi
Volume Resistivity
>10¹⁴ ohm-cm
  • RoHS Compliant
  • Bonding
  • Coating
  • Sealing
  • Gap Filling
  • Encapsulation
25,000-250,000 cps Cures rapidly upon exposure to LED light at 405 nm followed by heat curing at 90-95°C for 30-45 minutes 85-90 Shore D -80°F to +350°F /de/tds/led415dc90