EP42HT-2Med

Two component, high temperature resistant epoxy for medical device assembly; tested and approved for 3 medical related certifications

Key Features
  • ISO 10993-10 compliant for skin sensitization
  • USP Class VI approved
  • Passes ISO 10993-5 for cytotoxicity
  • Resists repeated sterilization, including autoclaving
Typical Properties
Viscosity
Part A: 55,000-110,000 cps, Part B: 30 - 70 CPS
Cure Schedule
overnight at 75°F followed by 2-4 hours at 150-250°F
Hardness
75-85 Shore D
Service Temperature Range
-60°F to 450°F
Acoustical Impedance
3.1 MRayl
Glass Transition Temperature (Tg)
150-155°C
Bild
EP42HT-2Med Two Part Epoxy
Product Description

Master Bond Polymer System EP42HT-2Med is a two component epoxy featuring convenient handling along with resistance to different types of repeated sterilization cycles. It has an easy to use 100 to 40 mix ratio by weight or 100 to 50 by volume. Some other features include good flow properties with moderate viscosity along with a long working life. It cures readily at ambient temperatures or more rapidly with heat. A number of cure schedule options are mentioned in the chart below, with the optimum being overnight at room temperature followed by 2-4 hours at 150-250°F. This system contains no solvents and has very low shrinkage upon curing.

EP42HT-2Med is an excellent adhesive and bonds well to a wide variety of substrates including metals, composites, ceramics, glass, as well as plastics and rubbers. It is highly resistant to acids, bases, solvents, and numerous sterilants. It is a top notch electrical and thermal insulator. Since it is a lower exothermic system, it can be used for encapsulation applications up to 3 inches deep. EP42HT-2Med is a higher Tg system with a service temperature range of -60°F to 450°F. The color of Part A is clear and Part B is amber clear. After curing, it transmits light very well. This is a “go to” type system for medical device manufacturing, especially for endoscopes, surgical instruments, and other devices that receive repeated sterilization.

Product Advantages

  • Convenient handling, good flow after mixing
  • Multi functional, for bonding, sealing, coating, potting
  • Highly resistant to radiation, EtO, and chemicals
  • Can withstand repeated steam autoclaving
  • Moderate acoustical impedance
  • USP Class VI, ISO 10993-5, ISO 10993-10 approved

Product Citation

EP42HT-2Med was cited in a paper titled "Fabrication and Packaging of a Fully Implantable Biosensor Array" by Camilla Baj-Rossi1, Enver G. Kilinc2, Sara S. Ghoreishizadeh1 , Daniele Casarino3 , Tanja Rezzonico Jost4, Catherine Dehollain2, Fabio Grassi4, Laura Pastorino3, Giovanni De Micheli1 and Sandro Carrara1. 1 Laboratory of Integrated Systems Swiss Federal Institute of Technology (EPFL), Lausanne, Switzerland 3 Universita degli Studi di Genova, Italy 4 Institute for Research in Biomedicine - IRB, Bellinzona, Switzerland For more information click here.

Show More

How to order

Verify Your Product Selection

With thousands of custom formulations available, our expert engineers provide personalized consultation to ensure you select the ideal adhesive. We will follow up with a product and packaging recommendation for your specific application.

Get a Quote

Our customer service team will follow up with a detailed quote with packaging and shipping options.

Place Your Order

We'll work with your company to process the order efficiently.

Receive Your Material

Your adhesive will be made to order and shipped to you. Typical lead times are 10-14 business days, with rush options available for urgent orders.