EP21LVFL
Two component, low viscosity epoxy for bonding, sealing, coating, and potting featuring good flexibility
Key Features
- Convenient handling
- High elongation
- Low modulus
- Withstands thermal cycling and shock
Typical Properties
Viscosity
10,000-14,000 cps
Cure Schedule
overnight at 75°F followed by 4-6 hours at 125-150°F
Hardness
40-50 Shore D
Service Temperature Range
-100°F to +250°F
Elongation
120-150%
Volume Resistivity
>10¹⁵ ohm-cm