EP21TDCAOHT
Two component epoxy compound for bonding, sealing and coating
Key Features
- Thermally conductive and electrically insulative
- Convenient handling
- Toughened system
- Higher temperature resistance
Typical Properties
Viscosity
Part A: 100,000-400,000 cps, Part B: paste
Cure Schedule
Optimum cure schedule: overnight at 75°F, plus 2-4 hours at 150-200°F.
Hardness
85-95 Shore D
Service Temperature Range
-100°F to +250°F
Coefficient of Thermal Expansion
21-24 X 10⁻⁶ in/in/°C
Tensile Lap Shear Strength
1,000-1,200 psi