EP21TDCHT-1
Toughened two component epoxy for bonding and sealing features high peel strength
Key Features
- Convenient processing, 1:1 mix ratio
- Superb strength profile
- Withstands aggressive thermal cycling
- Ideal for bonding dissimilar substrates
Typical Properties
Viscosity
Part A: 60,000-110,000 cps, Part B: 50,000-90,000 cps
Cure Schedule
overnight at ambient temperature followed by 60-90 minutes at 150-200°F
Hardness
60-70 Shore D
Service Temperature Range
-100°F to +400°F
Elongation
15-20%
T-peel Strength
20 pli
Tensile Lap Shear Strength
>2,400 psi
Tensile Modulus
200,000-250,000 psi
Volume Resistivity
>10¹⁴ ohm-cm
Bild
Discuss with a Specialist
(1-2 Business Day Request) Get Technical Data sheet
(Instant Email Delivery) Request Safety Data sheet
(1-2 Business Day Request)
(1-2 Business Day Request) Get Technical Data sheet
(Instant Email Delivery) Request Safety Data sheet
(1-2 Business Day Request)
Applications
Certifications
Meets EU Directive 2015/863