EP23

Highlight

Mineral Filled Two Component Epoxy Adhesive For High Performance Bonding And Sealing With Enhanced Dimensional Stability

Typical Properties
Bild
Product Description

Master Bond Polymer Adhesive EP23 is a mineral filled two component epoxy adhesive for high performance bonding formulated to cure at room temperature or more rapidly at elevated temperature with a one-to-one mix ratio, weight or volume. The EP23 adhesive develops high bonding strength of more than 2200 psi at room temperature which unlike that of many other epoxy adhesives, is relatively insensitive to mixing ratio or substrate cleaning procedures. Master Bond Polymer Adhesive EP23 produces durable and tough high strength bonds with outstanding adhesion to metals especially steel, iron and aluminum; ceramics; glass; wood; vulcanized rubber; and many plastics. The bonds feature remarkably high resistance to thermal cycling and chemicals including water, oil and most organic solvents, over the exceptionally wide temperature range of -60°F to more than 250°F. Color of part A tan, part B opaque tan. Master Bond EP23 adhesive is widely used in the electronic, electrical, computer, construction, metalworking, appliance, automotive and chemical industries.

Show More

How to order

Verify Your Product Selection

With thousands of custom formulations available, our expert engineers provide personalized consultation to ensure you select the ideal adhesive. We will follow up with a product and packaging recommendation for your specific application.

Get a Quote

Our customer service team will follow up with a detailed quote with packaging and shipping options.

Place Your Order

We'll work with your company to process the order efficiently.

Receive Your Material

Your adhesive will be made to order and shipped to you. Typical lead times are 10-14 business days, with rush options available for urgent orders.