EP29LPSPND-3
Two component epoxy compound for cryogenic applications
Key Features
- Paste consistency
- Exceptionally long working life
- Electrically and thermally insulative
- Can withstand cryogenic shock
Typical Properties
Viscosity
paste
Cure Schedule
Gel at 75°F for 12-24 hours followed by either option listed below: 130-150°F for 12-18 hours or 150-165°F for 5-10 hours.
Hardness
70-80 Shore D
Service Temperature Range
4K to 250°F
Dielectric Constant
4.2
Refractive Index
1.56