EP42HT-2FG Black
Two component, high temperature resistant epoxy for indirect food applications
Key Features
- Convenient processing
- Good physical strength properties
- Excellent chemical resistance properties
- Meets 175.105 food grade requirement
Typical Properties
Viscosity
Part A: 55,000-110,000 cps, Part B: 30-80 cps
Cure Schedule
overnight at 75°F followed by a post cure of 3-4 hours at 150-250°F
Hardness
80-90 Shore D
Service Temperature Range
-60°F to +450°F
Dielectric Constant
4.6
Glass Transition Temperature (Tg)
145-150°C
Bild
Discuss with a Specialist
(1-2 Business Day Request) Get Technical Data sheet
(Instant Email Delivery) Request Safety Data sheet
(1-2 Business Day Request)
(1-2 Business Day Request) Get Technical Data sheet
(Instant Email Delivery) Request Safety Data sheet
(1-2 Business Day Request)
Applications
Certifications
FDA Food Grade 21 CFR 175.105
Meets EU Directive 2015/863
Packaging