EP42HT-2HV1
Two component, room temperature curing epoxy compound featuring superior temperature and chemical resistance
Key Features
- Easy processing
- Cures at ambient or elevated temperatures
- Convenient working life
- High viscosity with good flow
Typical Properties
Viscosity
Part A: 130,000-170,000 cps, Part B: 30-70 cps
Cure Schedule
cures at ambient or elevated temperatures, with the optimum being overnight at 75°F followed by 2-4 hours at 150-200°F
Hardness
85-95 Shore D
Service Temperature Range
-60°F to +450°F
Dielectric Constant
3.8
Refractive Index
1.61
Volume Resistivity
>10¹⁴ ohm-cm