EP46CA-1
Two component epoxy for structural bonding featuring superlative heat resistance; requires oven curing
Key Features
- Long pot life at room temperature
- High bonding strength
- Service temperature range of -100°F to +500°F
- Outstanding electrical insulation properties
Typical Properties
Viscosity
5,000-20,000 cps
Cure Schedule
250-300°F for 2-3 hours, post cure for optimum properties at 350-400°F for 2 hours
Hardness
80-90 Shore D
Service Temperature Range
-100°F to +500°F
Dielectric Strength
450 volts/mil
Glass Transition Temperature (Tg)
160-170°C
Volume Resistivity
>10¹⁶ ohm-cm