MasterSil 981-LO

Two component silicone for bonding and sealing meets NASA low outgassing specifications

Key Features
  • High level of softness
  • Optically clear in thin sections
  • Addition cured
  • Convenient processing
Typical Properties
Viscosity
12,500-17,500 cps
Cure Schedule
Cures at ambient temperature in 48–72 hours, or more rapidly in 2–4 hours at 135–165°F. For optimal performance, an initial overnight cure at room temperature followed by 2–4 hours at 135–165°F is recommended.
Hardness
20-30 Shore A
Service Temperature Range
-65°F to +400°F
Coefficient of Thermal Expansion
450-500 x 10⁻⁶ in/in/°C
Refractive Index
1.437
Image
Two Part Silicone MasterSil 981-LO
Applications
Certifications

Meets EU Directive 2015/863

ASTM E595 Compliant

Product Description

Master Bond MasterSil 981-LO is a two-component silicone designed for high performance bonding, sealing, and encapsulating applications. It does not require air for curing. The system features a flowable viscosity and a forgiving 1:1 mix ratio by weight for ease of handling. It is a minimal exotherm material with an extended open time of approximately 3–4 hours. MasterSil 981-LO is also noteworthy for its soft Shore A hardness, offering a low modulus and good flexibility. MasterSil 981-LO cures at ambient temperature in 48–72 hours, or more rapidly in 2–4 hours at 135–165°F. For optimal performance, an initial overnight cure at room temperature followed by 2–4 hours at 135–165°F is recommended. The system is 100% reactive, containing no solvents or diluents, and exhibits minimal shrinkage upon cure.

MasterSil 981-LO bonds well to a wide range of substrates, including metals, glass, plastics, ceramics, and many types of silicone rubbers. It is capable of withstanding rigorous thermal shock and cycling without cracking or imparting stress on bonded components. The material has a Shore A hardness of 20–30 and a service temperature range of -65°F to +400°F. While tensile lap shear strength is relatively low, it still forms tenacious bonds and should be considered a reliable adhesive.

The color of both Parts A and B is clear. Additional key features include optical clarity, particularly in thinner sections, and a strong electrical insulation profile. MasterSil 981-LO is well suited for use in aerospace, satellite, optical, and optoelectronic applications where a low viscosity silicone with a long open time is required.

Show More

How to order

Verify Your Product Selection

With thousands of custom formulations available, our expert engineers provide personalized consultation to ensure you select the ideal adhesive. We will follow up with a product and packaging recommendation for your specific application.

Get a Quote

Our customer service team will follow up with a detailed quote with packaging and shipping options.

Place Your Order

We'll work with your company to process the order efficiently.

Receive Your Material

Your adhesive will be made to order and shipped to you. Typical lead times are 10-14 business days, with rush options available for urgent orders.