Supreme 121AOND
Two part toughened epoxy for bonding, sealing and encapsulation features good thermal conductivity
Key Features
- Paste consistency
- High temperature resistance
- Exceptionally long open time
- Passes NASA low outgassing
Typical Properties
Viscosity
paste
Cure Schedule
1-2 hours at 200-210°F followed by 3-4 hours at 250°F and then 4-6 hours at 300°F. Additional post curing at 350°F for 2-4 hours will enhance properties.
Hardness
85-95 Shore D
Service Temperature Range
-80°F to +550°F
Glass Transition Temperature (Tg)
200-210°C
Thermal Conductivity
4-5 BTU•in/(ft²•hr•°F)