Supreme 33
Toughened, two component epoxy for bonding, sealing and coating
Key Features
- Room temperature curing
- Convenient one to one mix ratio by volume
- Superior durability
- Thermal stabilty up to +425°F
- Withstands thermal cycling
- 100% reactive
Typical Properties
Cure Schedule
optimum cure is overnight at 75°F followed by a few hours at 150-200°F
Hardness
>75 Shore D
Service Temperature Range
-80°F to +425°F
Dielectric Strength
>400 volts/mil
Elongation
>75
Tensile Lap Shear Strength
>2,000 psi
Tensile Modulus
350,000-400,000 psi
Volume Resistivity
>10¹⁴ ohm-cm