UV15X-6NM-2BCL

Blue colored UV system for high performance bonding, sealing and coating, turns clear upon exposure to UV light
Key Features
  • Moderate viscosity
  • Outstanding abrasion resistance
  • Excellent flexibility and toughness
  • Good physical strength properties
Typical Properties
Viscosity
35,000-55,000 cps
Cure Schedule
UV light 320-365 nm for 30-60 seconds
Hardness
25-45 Shore D
Service Temperature Range
-80°F to +250°F
Dielectric Constant
4.5
Refractive Index
1.50
Image
UV Curable Adhesive System UV15X-6NM-2BCL
Certifications

Meets EU Directive 2015/863

Product Description

Master Bond UV15X-6NM-2BCL is a blue colored, moderate viscosity, one part UV curing urethane acrylate system. While curing, when the light reaches the UV material, it changes from blue to clear. However, if the the light does not reach the material, it remains blue. It should be noted that the color change does not indicate that full cure has been attained, but only that the UV light has reached the material.

The lamp should emit light with a wavelength range between 320-365 nm, the optimum being 365 nm. The typical energy required is 20-40 milliwatts per cm². Another variable is the distance of the light source from the material that is being cured. Taking into account these factors, full cure can generally be achieved in 30-60 seconds.

UV15X-6NM-2BCL is a free radical type curing system that is not oxygen inhibited and will cure in seconds up to 1/4 inch thick. It is most noteworthy for its inherent toughness and flexibility allowing it to resist severe thermal cycling as well as thermal and mechanical shocks. It contains no solvents and diluents and has very low shrinkage upon curing.

UV15X-6NM-2BCL bonds well to a variety of substrates including optically clear plastics such as polycarbonates and acrylics, composites, metals and many types of rubbers. It has good chemical resistance to water, oils, fuels, and cleaning agents. The system is thermally and electrically insulating with a service temperature range of -80°F to +250°F. Upon curing, it has superior non-yellowing resistance. This UV curable system can be used in fiber-optic, optical, electronic, semiconductor, microelectronic and laser applications, especially when thermal cycling is a significant consideration in the application.

Product Advantages

  • Free radical cure but not oxygen inhibited
  • Reliable thermal and electrical insulator
  • Outstanding flexibility and toughness
  • Good abrasion resistance
  • Resists thermal cycling and shock
Show More

How to order

Verify Your Product Selection

With thousands of custom formulations available, our expert engineers provide personalized consultation to ensure you select the ideal adhesive. We will follow up with a product and packaging recommendation for your specific application.

Get a Quote

Our customer service team will follow up with a detailed quote with packaging and shipping options.

Place Your Order

We'll work with your company to process the order efficiently.

Receive Your Material

Your adhesive will be made to order and shipped to you. Typical lead times are 10-14 business days, with rush options available for urgent orders.