UV16Med

Low viscosity, medical grade UV curable epoxy based system for bonding, sealing and coating
Key Features
  • Cationic curing, no oxygen inhibition
  • Low shrinkage upon curing
  • Good physical strength properties
  • Passes ISO 10993-5
Typical Properties
Viscosity
250-500 cps
Cure Schedule
UV light 320-365 nm for 20-30 seconds
Hardness
70-80 Shore D.
Service Temperature Range
-80°F to +400°F.
Dielectric Constant
3.1
Glass Transition Temperature (Tg)
90-95°C without post cure; 135-140°C with post cure.
Bild
Certifications

ISO 10993-5 for Cytotoxicity

Meets EU Directive 2015/863

Product Description

Master Bond UV16Med is a low viscosity, high strength epoxy based UV curable system for bonding, sealing and coating. It is 100% reactive and does not contain any solvents or other volatiles. It is a cationic curing system and has no oxygen inhibition. UV16Med cures quickly when exposed to a UV light source with a wavelength ranging between 320-365 nm, with the optimum at 365 nm. The energy required is typically 20-40 milliwatts per cm². The rate of cure depends upon the distance of the light from the material being cured, the thickness of the section and the intensity of the light source. It typically cures in thicknesses of 0.001-0.002 inches up to 0.120 inches, with thinner sections generally curing in 30-60 seconds. Thicker sections will take longer to cure, and post curing with heat will enhance the cured properties.

UV16Med bonds well to a wide variety of substrates including plastics, glass and many metals. It is highly resistant to acids, bases, solvents, and numerous sterilants, including ethylene oxide and gluteraldehyde. It also withstands repeated autoclaving. The chemistry of the cured system allows for good thermal cycling capabilities. It is a reliable thermal and electrical insulator with a service temperature range of -80°F to +400°F.

Since UV16Med is a cationic curing system, it has a higher glass transition temperature compared to other UV type systems. Post curing with heat is required in achieving a higher Tg. Without heating, the Tg is 90-100°C. If post cured for 30 minutes at 125°C, the Tg increases to about 130-135°C. Additional post curing at this temperature will further increase the Tg allowing for better resistance to autoclaving. UV16Med is an attractive candidate in medical applications where UV light curing is feasible and resistance to sterilization is critical.

Product Advantages

  • One part system
  • Not oxygen inhibited
  • Outstanding optical clarity
  • Can resist repeated autoclaving
  • Passes ISO 10993-5 for cytotoxicity
Show More

How to order

Verify Your Product Selection

With thousands of custom formulations available, our expert engineers provide personalized consultation to ensure you select the ideal adhesive. We will follow up with a product and packaging recommendation for your specific application.

Get a Quote

Our customer service team will follow up with a detailed quote with packaging and shipping options.

Place Your Order

We'll work with your company to process the order efficiently.

Receive Your Material

Your adhesive will be made to order and shipped to you. Typical lead times are 10-14 business days, with rush options available for urgent orders.