UV23FLDC-80TK
One component, UV and heat curable epoxy system with moderate viscosity that cures with good flexibility
Key Features
- Cures in shadowed out areas with heat
- Curing temperature 80-85°C
- Excellent elongation
- Outstanding thermal cycling properties
Typical Properties
Viscosity
25,000-50,000 cps
Cure Schedule
initial cure utilizing UV light along with secondary curing in shadowed out areas by heating, typically 60-90 minutes at 80-85°C
Hardness
45-55 Shore D
Service Temperature Range
-80°F to +300°F
Dielectric Constant
4.7
Elongation
90-100% at 75°F
Bild
Discuss with a Specialist
(1-2 Business Day Request) Get Technical Data sheet
(Instant Email Delivery) Request Safety Data sheet
(1-2 Business Day Request)
(1-2 Business Day Request) Get Technical Data sheet
(Instant Email Delivery) Request Safety Data sheet
(1-2 Business Day Request)
Applications
Certifications
Meets EU Directive 2015/863