Master Bond Test Results
Testing Adhesives for Resistance to DMSO
 
 
 
 
 
 
Master Bond tested epoxies from our line of chemically resistant compounds for their ability to resist exposure to DMSO (dimethyl sulfoxide). Ten of our top performing compounds were cured and then immersed in DMSO (some for over a 2.5 year span) while weekly measurements were recorded to assess the percentage of weight change from start to finish. See the results of our best performing DMSO resistant adhesives.
Top Adhesive Systems with DMSO Resistance
 
 
 
Master Bond Product EP46HT-2AO Black
EP46HT-2AO Black
Two part, NASA low outgassing approved epoxy system
Request a Technical Datasheet
Master Bond Product EP62-1HT
EP62-1HT
Moderate viscosity epoxy for bonding and coating applications
Request a Technical Datasheet
Master Bond Product UV25
UV25
UV curable system with high glass transition temperature
Request a Technical Datasheet
Master Bond Product EP125
EP125
Flexible, two part epoxy resists prolonged exposure above 500°F
Request a Technical Datasheet
Master Bond Facebook Master Bond LinkedIn Master Bond Twitter Master Bond LinkedIn

Master Bond Inc. | www.masterbond.com | [email protected] | +1.201.343.8983
154 Hobart Street, Hackensack, New Jersey 07601 USA


Copyright © 2023 by Master Bond Inc. All Rights Reserved.
This content may not be reproduced in any way without the prior written permission of Master Bond Inc.