Master Bond Test Results
Testing Adhesive Compounds for Resistance to Acetone
 
 
 
 
 
 
Master Bond tested a variety of epoxy formulations for their resistance to acetone. Cured samples of epoxy were immersed over a long period of time in acetone and weight changes were recorded weekly. View the results of the tested compounds and see which performed best.
Acetone Resistant Adhesive Systems
 
 
 
Master Bond Product EP41S-1HT
EP41S-1HT
Two part epoxy with impressive physical strength properties
Request a Technical Datasheet
Master Bond Product EP41S-5LV
EP41S-5LV
Epoxy with superior electrical insulation properties
Request a Technical Datasheet
Master Bond Product EP62-1HT
EP62-1HT
Moderate viscosity epoxy for bonding and coating applications
Request a Technical Datasheet
Master Bond Product EP46HT-2AO Black
EP46HT-2AO Black
Two part, NASA low outgassing approved epoxy system
Request a Technical Datasheet
Master Bond Product UV25
UV25
UV curable system with high glass transition temperature
Request a Technical Datasheet
Master Bond Facebook Master Bond LinkedIn Master Bond Twitter Master Bond LinkedIn

Master Bond Inc. | www.masterbond.com | [email protected] | +1.201.343.8983
154 Hobart Street, Hackensack, New Jersey 07601 USA


Copyright © 2022 by Master Bond Inc. All Rights Reserved.
This content may not be reproduced in any way without the prior written permission of Master Bond Inc.