Master Bond Inc.
Having trouble viewing images? View email in browser
Master Bond Test Results
Testing Adhesives for Resistance to Acetonitrile
 
 
 
 
 
 
Master Bond tested select chemically resistant epoxies and UV curing systems for their resistance to acetonitrile. Thin castings of each material were immersed in acetonitrile over a span of 10 months to over 2.5 years while the percentage of weight change was recorded from start to finish. See the performance data for different adhesive compounds.
Top Acetonitrile Resistant Adhesive Systems
 
 
 
Master Bond Product EP41S-5
EP41S-5
Electrically insulative epoxy ideal for coating tanks & vessels
Request a Technical Datasheet
Master Bond Product EP46HT-2AO Black
EP46HT-2AO Black
Two part, NASA low outgassing approved epoxy system
Request a Technical Datasheet
Master Bond Product EP41S-5LV
EP41S-5LV
Epoxy system featuring superior electrical insulation
Request a Technical Datasheet
Master Bond Product EP62-1HT
EP62-1HT
Moderate viscosity epoxy for bonding and coating applications
Request a Technical Datasheet
Master Bond Product UV25
UV25
UV curable system with high glass transition temperature
Request a Technical Datasheet
Master Bond Product EP41S-1HT
EP41S-1HT
Two part epoxy with impressive physical strength properties
Request a Technical Datasheet
Master Bond Facebook Master Bond LinkedIn Master Bond Twitter Master Bond LinkedIn

Master Bond Inc. | www.masterbond.com | [email protected] | +1.201.343.8983
154 Hobart Street, Hackensack, New Jersey 07601 USA


Copyright © 2023 by Master Bond Inc. All Rights Reserved.
This content may not be reproduced in any way without the prior written permission of Master Bond Inc.