Master Bond Test Results
Testing Adhesives for Resistance to Ethanol
 
 
 
 
 
 
Master Bond offers a full line of chemical resistant epoxies and UV curable systems. Select compounds have recently been tested for their efficiency in resisting Ethanol. By immersing thin cured castings into the Ethanol fluid over a span of 37 weeks and recording the weight change of the castings weekly, it was determined which products were most effective in resisting exposure to Ethanol. See what the results have to say and which materials worked best.
Ethanol Resistant Adhesives
 
 
 
Master Bond Product EP41S-5
EP41S-5
High strength, two part epoxy with moderate viscosity
Request a Technical Datasheet
Master Bond Product EP62-1HT
EP62-1HT
Low viscosity epoxy with high temperature resistance
Request a Technical Datasheet
Master Bond Product UV25
UV25
UV curable adhesive with high glass transition temperature
Request a Technical Datasheet
Master Bond Product EP46HT-2AO Black
EP46HT-2AO Black
Low outgassing epoxy with excellent dimensional stability
Request a Technical Datasheet
Master Bond Facebook Master Bond LinkedIn Master Bond Twitter Master Bond LinkedIn

Master Bond Inc. | www.masterbond.com | [email protected] | +1.201.343.8983
154 Hobart Street, Hackensack, New Jersey 07601 USA


Copyright © 2019 by Master Bond Inc. All Rights Reserved.
This content may not be reproduced in any way without the prior written permission of Master Bond Inc.