Testing Adhesives for Resistance to Phosphoric Acid
 
 
 
 
 
 
Master Bond has thoroughly tested specific epoxy compounds for phosphoric acid resistance, emphasizing their superior durability and performance. These epoxies undergo rigorous exposure to varying phosphoric acid concentrations, demonstrating significantly greater resistance and minimal degradation compared to conventional epoxies ensuring their effectiveness in demanding chemical environments.
Phosphoric Acid Resistant Epoxies
 
 
 
Master Bond Product EP62-1HT
EP62-1HT
Low outgassing, high strength epoxy with long working life
Request a Technical Datasheet
Master Bond Product EEP62-1BF
EP62-1BF
Lower viscosity epoxy for potting small components
Request a Technical Datasheet
Master Bond Product EP41S-5
EP41S-5
Electrically insulative epoxy ideal for coating tanks & vessels
Request a Technical Datasheet
Master Bond Product EP21ARHT
EP21ARHT
Epoxy with high bond strength to both similar and dissimilar substrates
Request a Technical Datasheet
Master Bond Product EP17HT
EP17HT
Serviceable up to 600°F, retains performance properties at high temperatures
Request a Technical Datasheet
Master Bond Product EP125
EP125
Structural epoxy with exceptional durability and flexural strength
Request a Technical Datasheet
Master Bond Product EP35SP
EP35SP
Epoxy features high Tg and wide service temperature range
Request a Technical Datasheet
Master Bond Product EP46HT-1
EP46HT-1
Heat resistant epoxy with outstanding electrical insulation
Request a Technical Datasheet
Master Bond Facebook Master Bond LinkedIn Master Bond Twitter Master Bond LinkedIn

Master Bond Inc. | www.masterbond.com | [email protected] | +1.201.343.8983
154 Hobart Street, Hackensack, New Jersey 07601 USA


Copyright © 2024 by Master Bond Inc. All Rights Reserved.
This content may not be reproduced in any way without the prior written permission of Master Bond Inc.