Master Bond Test Results
Testing Adhesive Compounds for Resistance to Xylene
 
 
 
 
 
 
Master Bond’s tech experts tested our highly rated, chemically resistant compounds for their ability to withstand xylene. Using a variety of two part epoxies and one part UV curing compounds, cured samples were immersed in the chemical and weekly measurements were recorded – with some products staying immersed for over a span of 2.5 years! See the results of our best performing epoxies and UV curing systems for xylene resistance.
Xylene Resistant Adhesive Systems
 
 
 
Master Bond Product EP41S-5
EP41S-5
Electrically insulative epoxy ideal for coating tanks & vessels
Request a Technical Datasheet
Master Bond Product EP62-1HT
EP62-1HT
Moderate viscosity epoxy for bonding and coating applications
Request a Technical Datasheet
Master Bond Product EP42HT-2AO-1 Black
EP42HT-2AO-1 Black
Cryogenically serviceable epoxy castable up to 3 inches thick
Request a Technical Datasheet
Master Bond Product UV22DC80-1
UV22DC80-1
One part UV and heat curing nanosilica filled adhesive
Request a Technical Datasheet
Master Bond Product UV25
UV25
UV curable system with high glass transition temperature
Request a Technical Datasheet
Master Bond Facebook Master Bond LinkedIn Master Bond Twitter Master Bond LinkedIn

Master Bond Inc. | www.masterbond.com | [email protected] | +1.201.343.8983
154 Hobart Street, Hackensack, New Jersey 07601 USA


Copyright © 2022 by Master Bond Inc. All Rights Reserved.
This content may not be reproduced in any way without the prior written permission of Master Bond Inc.