Master Bond Test Results
Testing Epoxies for Resistance to Sulfuric Acid
 
 
 
 
 
 
Master Bond tested epoxies from our line of chemically resistant compounds for their ability to resist sulfuric acid. Cured samples of 5 of our top performing compounds were immersed in a 98% solution of sulfuric acid over a span of 6 months while weekly measurements were recorded to assess the percentage of weight change from start to finish. See the results of our best performing epoxies for resistance to sulfuric acid.
Sulfuric Acid Resistant Adhesive Systems
 
 
 
Master Bond Product EP62-1HT
EP62-1HT
Moderate viscosity epoxy for bonding and coating applications
Request a Technical Datasheet
Master Bond Product EP62-1BF
EP62-1BF
Rapid curing, two part epoxy with high Tg of 170-175°C
Request a Technical Datasheet
Master Bond Product EP41S-5
EP41S-5
Electrically insulative epoxy ideal for coating tanks & vessels
Request a Technical Datasheet
Master Bond Product EP21ARHT
EP21ARHT
Epoxy resists high temperatures and offers low shrinkage
Request a Technical Datasheet
Master Bond Product EP35SP
EP35SP
Paste viscosity epoxy serviceable from -80°F to +550°F
Request a Technical Datasheet
Master Bond Facebook Master Bond LinkedIn Master Bond Twitter Master Bond LinkedIn

Master Bond Inc. | www.masterbond.com | [email protected] | +1.201.343.8983
154 Hobart Street, Hackensack, New Jersey 07601 USA


Copyright © 2023 by Master Bond Inc. All Rights Reserved.
This content may not be reproduced in any way without the prior written permission of Master Bond Inc.